Access a comprehensive, professionally formatted Material Test Certificate according to EN 10204-2004: 3.1 for ASTM A193 Grade B6. Review the rigorous documentation verifying this 12% Chromium martensitic stainless steel's chemistry, specialized heat treatments, and mechanical strength intended for high-temperature pressure vessels and highly corrosive environments.
This sample mill test certificate emphasizes the key testing parameters required for ASTM A193 Grade B6—a high-strength, martensitic stainless steel (similar to AISI 410) chosen for its excellent balance of mechanical strength and resistance to scaling/oxidation up to 1200°F (650°C).
Review the standard parameters and layout before downloading the full document.
TC Number
S95/26-XX
TC Date
22.09.20XX
Material Spec
ASTM A193 GRADE B6
Bar Shape / Size
Round Bar / 22 mm
Dimensions / Item
Stud Bolt M22-2.5P x 150 mm
Quantity
40.00 NOS
| C | Mn | P | S | Si | Cr |
|---|---|---|---|---|---|
| 0.12 | 0.45 | 0.020 | 0.015 | 0.30 | 12.50 |
| Max: 0.15 | Max: 1.00 | Max: 0.040 | Max: 0.030 | Max: 1.00 | Min: 11.50 Max: 13.50 |
| TENSILE STRENGTH (MPa) | YIELD STRENGTH 0.2% Offset (MPa) | % ELONGATION (GL-50mm) | HARDNESS (HBW) |
|---|---|---|---|
| 810.50 | 645.20 | 20.50 | 265, 268, 266 |
| Min: 760 (110 ksi) | Min: 585 (85 ksi) | Min: 15 | Max: 321 |
Our MTC certificates comprehensively align with the demanding specifications of the power generation and chemical processing sectors. The test reports confirm exact compliance with ASME/ASTM A193 / A193M Grade B6 with respect to the specific heat and lot tested.
| Standard / Requirement | Confirmation on Certificate |
|---|---|
| Visual Inspection | 100% visual inspection carried out & found free from defects. |
| Safety Requirements | Material is free from radioactive contamination and mercury. |
| Weld Repairs | No weld repair performed. |
| Dimensional Accuracy | All Dimensions are as per PO Specification / ASME B18.2.1 / B18.2.2. |
We confirm that the above mentioned items were Manufactured, Sampled, Tested, and Inspected in accordance with the subjected Customer's Purchase Order and applicable Drawings, Material Specifications, Codes & Standards.
The 12% Chromium content places Grade B6 in the martensitic stainless steel family. This specific chemistry provides an outstanding balance—it is highly hardenable for excellent tensile strength, while still offering robust resistance to oxidation and corrosion from steam, hot gases, and mild acids.
Martensitic stainless steels can become brittle if tempered improperly. The ASTM A193 specification dictates a minimum tempering temperature of 1100°F (593°C) to ensure the fasteners achieve the required ductility and toughness while relieving internal quenching stresses, making them safe for pressurized service.
While both are made from Type 410 stainless steel, they have different mechanical requirements. Grade B6 has a higher minimum tensile strength (110 ksi) and yield strength (85 ksi). Grade B6X requires a lower minimum tensile strength (90 ksi) and yield strength (70 ksi) but mandates a higher minimum tempering temperature (1200°F / 650°C), usually for applications prioritizing greater ductility over maximum strength.