ASTM A193 B7M Bolts and Studs: B7 vs B7M, Hardness and Sour Service
ASTM A193 B7M (A193 Gr B7M) is the hardness-controlled version of B7. It has the same chromium-molybdenum chemistry, but it is tempered hotter so that hardness stays at or below 235 HBW (99 HRB). That makes B7M bolts and B7M studs the standard choice for sour-service flanges, wellhead and valve bolting, always paired with A194 Grade 2HM nuts.
| Specification | ASTM A193/A193M, Grade B7M |
|---|
| Material | Cr-Mo alloy steel, same chemistry as B7 |
|---|
| Min temper | 1150 °F (620 °C) |
|---|
| Tensile / yield (≤ 4 in) | 100 ksi (690 MPa) / 80 ksi (550 MPa) min |
|---|
| Hardness | 200 – 235 HBW (93 – 99 HRB) |
|---|
| Mating nut | ASTM A194 Grade 2HM |
|---|
Request a Quote
■ B7 vs B7M: the difference between B7 and B7M bolts
If you only remember one thing: B7M gives up strength for a hardness ceiling. The steel is the same, the tempering is hotter, and the hardness window is narrower.
| Property | A193 B7 | A193 B7M |
|---|
| Chemistry | Cr-Mo (4140 family) | Same as B7 |
| Min tempering temperature | 1100 °F (593 °C) | 1150 °F (620 °C) |
| Min tensile, ≤ 2½ in | 125 ksi (860 MPa) | 100 ksi (690 MPa) |
| Min yield, ≤ 2½ in | 105 ksi (720 MPa) | 80 ksi (550 MPa) |
| Hardness | 321 HBW / 35 HRC max | 200 – 235 HBW (93 – 99 HRB) |
| Mating nut (A194) | Grade 2H | Grade 2HM |
| Hardness testing | Per specification sampling | Each piece tested (S3 asks for 100 % indentation) |
| Typical use | General high-temperature and high-pressure bolting | Sour service and hardness-limited joints |
| Marking | B7 | B7M |
*Source: ASTM A193/A193M, Tables for B7 and B7M, with A194 nut pairing per ASME B16.5. Confirm against the edition on your purchase order.
B7M is not a drop-in upgrade. Because its minimum yield and tensile strength are lower than B7, the allowable stress and achievable preload are lower too. Only the design engineer can approve replacing B7 with B7M.
■ B7M chemical composition
B7M uses the same chemistry limits as B7.
| Element | Heat analysis (B7 and B7M), wt % | Product analysis tolerance |
|---|
| Carbon (C) | 0.38 – 0.48 | ± 0.02 |
| Manganese (Mn) | 0.75 – 1.00 | ± 0.04 |
| Phosphorus (P) | 0.035 max | + 0.005 |
| Sulfur (S) | 0.040 max | + 0.005 |
| Silicon (Si) | 0.15 – 0.35 | ± 0.02 |
| Chromium (Cr) | 0.80 – 1.10 | ± 0.05 |
| Molybdenum (Mo) | 0.15 – 0.25 | ± 0.02 |
*AISI 4140, 4142, 4145 and the corresponding H grades are permitted. For bar over 3½ in, carbon up to 0.50 % is allowed. Source: ASTM A193/A193M chemical requirements table and its footnotes. Confirm against the edition on your purchase order. For B7M, 4130 steel (carbon 0.28 % minimum) may be used if the tensile requirement is met.
■ B7M mechanical properties
| Diameter | Min tensile | Min yield (0.2 %) | Min elongation | Min reduction of area | Hardness |
|---|
| ≤ 4 in (≤ M100) | 100 ksi (690 MPa) | 80 ksi (550 MPa) | 18 % | 50 % | 200 – 235 HBW (93 – 99 HRB) |
| > 4 to 7 in (M100 – M180) | 100 ksi (690 MPa) | 75 ksi (515 MPa) | 18 % | 50 % | 200 – 235 HBW (93 – 99 HRB) |
*Source: ASTM A193/A193M mechanical requirements for Grade B7M. Minimum tempering temperature 1150 °F (620 °C).
Note that B7M uses one size break at 4 in, whereas B7 has breaks at 2½ in and 4 in.
■ B7M bolts material in sour service
In wet H2S environments, hard steel can crack suddenly under stress (sulfide stress cracking). Limiting hardness is the main way bolting is protected. NACE MR0175 / ISO 15156 sets 22 HRC as the ceiling for carbon and low-alloy bolting, and ASTM A193 B7M with A194 2HM nuts is the combination those standards recognise for this duty.
- A193 states the B7M limit as 235 HBW or 99 HRB. The 22 HRC figure is the NACE ceiling: keep the units separate on drawings and certificates.
- Low hardness reduces the risk but does not remove it: the environment limits in ISO 15156 (H2S partial pressure, pH, temperature, chlorides) still apply.
- Verify the edition of ISO 15156-2 named in your project specification.
■ How B7M bolts are made and tested
- Heat treatment: liquid quench and temper at 1150 °F (620 °C) minimum.
- Order of operations: final heat treatment comes after all machining and thread rolling, so rolled-thread cold work cannot push hardness above the limit.
- Hardness testing: A193 requires each B7M piece to be tested. An electromagnetic method may be used if it is qualified against indentation testing on a sample. Supplementary requirement S3 raises this to 100 % indentation testing.
- Marking: "B7M" (underlining optional), with the manufacturer mark per A962. Zinc-coated parts carry "ZN" after the grade symbol.
■ Nuts for B7M studs
B7M studs and bolts are paired with ASTM A194 Grade 2HM heavy hex nuts: 22 HRC maximum, 159 to 237 HB. Ordering a standard 2H nut with B7M bolting is a common specification error because 2H can be harder than the sour-service limit. Our A194 nut range includes 2H and 2HM.
■ How to order B7M studs: checklist
- State "ASTM A193/A193M Grade B7M" and the edition required.
- Product form, diameter, thread series and class, and length.
- Nut grade: ASTM A194 Grade 2HM.
- Hardness reporting: actual HBW or HRB on the certificate for each lot, and S3 if 100 % indentation testing is required.
- Sour-service standard and edition (NACE MR0175 / ISO 15156) if applicable.
- Coating and temperature limit, if any.
- EN 10204 3.1 certificate, with heat-treatment record.
■ A193 B7M FAQ
1. What is ASTM A193 B7M?
ASTM A193 Grade B7M is a chromium-molybdenum alloy steel bolting grade with the same chemistry as B7 but tempered at a minimum of 1150 °F (620 °C) to a controlled hardness of 235 HBW or 99 HRB maximum (minimum 200 HBW or 93 HRB). It is used where hardness must be limited, mainly in sour (H2S) service.
2. What is the difference between B7 and B7M bolts?
The chemistry is the same. B7M is tempered hotter and held to a hardness range of 200 to 235 HBW, so its minimum tensile strength is 100 ksi (690 MPa) against 125 ksi (860 MPa) for B7 up to 2½ in. B7 reaches up to 321 HBW. B7M pairs with A194 Grade 2HM nuts and B7 with Grade 2H.
3. Can B7M replace B7?
Not automatically. B7M has lower minimum tensile and yield strength than B7, so the joint's allowable stress and preload may change. A substitution needs sign-off from the design engineer. Going the other way, B7 should not be used in sour service unless the project specification allows it, because its hardness can exceed the limit.
4. Which nut do I use with A193 B7M?
Use ASTM A194 Grade 2HM heavy hex nuts. Grade 2HM is hardness controlled (22 HRC maximum, 159 to 237 HB) for sour service. Grade 2H is the nut for B7.
5. Is B7M suitable for sour service?
B7M is the standard bolting grade chosen for sour service because its low hardness reduces the risk of sulfide stress cracking. Compliance is not automatic: NACE MR0175 / ISO 15156 limits carbon and low-alloy bolting to 22 HRC and also limits the environment. A193 expresses the B7M limit as 235 HBW or 99 HRB, so keep the units separate and confirm the edition of ISO 15156 your project cites.
6. Why must B7M be heat treated after threading?
A193 requires the final heat treatment of B7M to follow all machining and thread rolling. Cold work from rolling threads raises hardness, and a later temper restores it to within the 235 HBW limit. A193 also requires hardness testing of each B7M piece, with an electromagnetic method allowed if it is qualified against indentation testing, and supplementary requirement S3 asks for 100 % indentation testing.
7. Is B7M the same as 4140?
No. AISI 4140, 4142 and 4145 are permitted starting steels, and 4130 may be used for B7M if the tensile requirement is met, but the grade is defined by heat treatment and tested properties, not by the steel designation alone.
■ Related guides
ASTM A193 fasteners: all grades | ASTM A193 B7 | ASTM A194 2H / 2HM nuts
Send your size list, sour-service standard and hardness reporting needs and we will quote A193 B7M studs with matching 2HM nuts.